Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Ultramid® T KR 4365 G5 - PA6T/6-GF25 FR(52) - BASF

Material Data Center offers the following functions for Ultramid® T KR 4365 G5:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, parameters for material models, CAE Interfaces

Check here, which other Ultramid T datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Testo del prodotto
A glass fibre reinforced, flame retardant, partially aromatic polyamide for injection molding. Good mechanical properties, low water absorption, high melting point (295°C). High tracking resistance, low tendency to form deposits on electrical contacts, very resistant to electrolytic corrosion, resistant to soldering temperatures, can be electroplated.
Caratteristiche Fisichesecco/condUnitáNorma del test
ISO Data
Ritiro di stampaggio, parallelo 0.6 / * % ISO 294-4, 2577
Ritiro di stampaggio, perpendicolare 1.0 / * % ISO 294-4, 2577
Proprietà Meccanichesecco/condUnitáNorma del test
ISO Data
Modulo a trazione 8300 / 8000 MPa ISO 527
Carico unitario a rottura 150 / - MPa ISO 527
Deformazione a rottura 3 / - % ISO 527
Modulo di scorrimento a trazione, 1000h * / 6400 MPa ISO 899-1
Resistenza all'urto Charpy, +23°C 70 / 55 kJ/m² ISO 179/1eU
Resistenzia all'urto Charpy con intaglio, +23°C 8 / 7 kJ/m² ISO 179/1eA
Proprietà Termichesecco/condUnitáNorma del test
ISO Data
Temperatura di fusione, 10°C/min 295 / * °C ISO 11357-1/-3
Temperatura di transizione vetrosa, 10°C/min 105 / * °C ISO 11357-1/-2
Temp.di inflessione sotto carico, 1.80 MPa 220 / * °C ISO 75-1/-2
Temp.di rammollimento Vicat, B 285 / * °C ISO 306
Coeff.di dilatazione termica lin., parallelo 24 / * E-6/K ISO 11359-1/-2
Coeff.di dilatazione termica lin., perpend. 67 / * E-6/K ISO 11359-1/-2
Reaz. al fuoco spess.nom. 1.5mm V-0 / * class IEC 60695-11-10
Spessore provato 1.6 / * mm -
Yellow Card disponibile sì / * - -
Reazione al fuoco a spessore h V-0 / * class IEC 60695-11-10
Spessore provato 0.8 / * mm -
Yellow Card disponibile sì / * - -
Reazione al fuoco 5V a spess. h 5VA / * class IEC 60695-11-20
Spessore provato 1.5 / * mm -
Yellow Card disponibile sì / * - -
Indice di ossigeno 26 / * % ISO 4589-1/-2
Proprietà Elettrichesecco/condUnitáNorma del test
ISO Data
Costante dielettrica relativa, 1MHz 4 / - - IEC 62631-2-1
Fattore di dissipazione, 1MHz 200 / - E-4 IEC 62631-2-1
Resistività volumica 1E13 / 1E12 Ohm*m IEC 62631-3-1
Resistività superficiale * / 1E14 Ohm IEC 62631-3-2
Rigidità dielettrica 37 / 33 kV/mm IEC 60243-1
Res. Alle correnti striscianti superficiali - / 600 - IEC 60112
Altre Proprietàsecco/condUnitáNorma del test
Assorbimento d'acqua 5.5 / * % Sim. alla ISO 62
Assorbimento d'umidità 1.3 / * % Sim. alla ISO 62
Massa volumica 1380 / - kg/m³ ISO 1183
Proprietà Specifiche Materialesecco/condUnitáNorma del test
ISO Data
Numero di viscosità 130 / * cm³/g ISO 307, 1157, 1628
Raccomandazione de Processabilità Stampaggio ad IniezioneValoreUnitáNorma del test
Pre-essiccamento - Temperatura 110 °C -
Pre-essiccamento - Tempo 8 h -
Temperatura di fusione 310 - 330 °C -
Temperatura dello stampo 80 - 120 °C -
Funzioni
Modulo dinamico a taglio-temperatura , Ultramid® T KR 4365 G5 (Secco), PA6T/6-GF25 FR(52), BASF
Sforzi-deformazione , Ultramid® T KR 4365 G5 (Secco), PA6T/6-GF25 FR(52), BASF
Sforzi-deformazione , Ultramid® T KR 4365 G5 (cond.), PA6T/6-GF25 FR(52), BASF
Modulo secante-deformazione , Ultramid® T KR 4365 G5 (Secco), PA6T/6-GF25 FR(52), BASF
Modulo secante-deformazione , Ultramid® T KR 4365 G5 (cond.), PA6T/6-GF25 FR(52), BASF
Sforzi-deformazioni (isocrona) 23°C, Ultramid® T KR 4365 G5 (cond.), PA6T/6-GF25 FR(52), BASF
Modulo di scorrimento-tempo 23°C, Ultramid® T KR 4365 G5 (cond.), PA6T/6-GF25 FR(52), BASF
Curva di scorrimento 23°C, Ultramid® T KR 4365 G5 (cond.), PA6T/6-GF25 FR(52), BASF
Sforzi-deformazioni (isocrona) 120°C, Ultramid® T KR 4365 G5 (Secco), PA6T/6-GF25 FR(52), BASF
Modulo di scorrimento-tempo 120°C, Ultramid® T KR 4365 G5 (Secco), PA6T/6-GF25 FR(52), BASF
Curva di scorrimento 120°C, Ultramid® T KR 4365 G5 (Secco), PA6T/6-GF25 FR(52), BASF
Modulo a taglio-temperatura , Ultramid® T KR 4365 G5 (Secco), PA6T/6-GF25 FR(52), BASF
Modulo a taglio-temperatura , Ultramid® T KR 4365 G5 (cond.), PA6T/6-GF25 FR(52), BASF
Caratteristiche
Processabilità e Forma di Forni
Stampaggio ad Iniezione
Forma fisica disponibile
Pellet
Additivi
Agente di distacco
Caratteristiche speciali
Ritardante di fiamma, Senza alogeni, Stabilizzato o stabile al calore
Disponibilità geografica
Altre informazioni
Stampaggio ad Iniezione
PREPROCESSING
Pre/Post-processing, Pre-drying, Temperature: 110 °C
Pre/Post-processing, Pre-drying, Time: 8 h

PROCESSING
injection molding, Melt temperature, range: 310 - 330 °C
injection molding, Melt temperature, recommended: 320 °C
injection molding, Mold temperature, range: 80 - 120 °C
injection molding, Mold temperature, recommended: 100 °C
injection molding, Dwell time, thermoplastics: 5 min
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.